Austenitic steels

TP 321H • UNS S32100 • 1.4878 • TPS-INOX 4878-321H

Datasheet

This is the high carbon version of TP 321 which ensures greater creep resistance. Behaves much the same as TP 321 in oxidation resistance. Main applications: Heat exchangers, furnaces, boilers in chemical and petrochemical plant.

Chemical composition • mass in %

Material grade Norm C
max.
Si
max.
Mn
max.
P
max.
S
max.
Cr Ni Mo Ti others
1.4878 EN 10297-2 0,100 1,00 2,00 0,045 0,015 17,00 - 19,00 9,00 - 12,00 5x% C max. 0,70
TP321H ASME SA / ASTM A 213 0,040 - 0,100 1,00 2,00 0,040 0,030 17,00 - 19,00 9,00 - 12,00 5x% C max. 0,70

Mechanical properties and heat treatment

Material grade Norm Rp 0,2 MPa
min.
Rp 1,0 MPa
min.
Rm MPa
min. max.
A
min.%
Hardness
HRB max.
Heat treatment
1.4878 EN 10297-2 190 230 500 40 solution annealed
TP321H ASME SA / ASTM A 213 205 515 35 90 solution annealed

Rp 0,2 = Rotation

Rp 1,0 = Yield Strength

Rm = Tensile Strength

A = Elongation

Tolerances

OD - Tube OD WT special WT ID
ab Ø4,55 mm ±0,050 mm ±0,150 mm ±0,100 mm X
ab Ø9,53 mm ±0,050 mm ±0,100 mm ±0,080 mm ±0,050 mm
ab Ø30,00 mm ±0,100 mm ±0,150 mm ±0,050 mm

Scope of dimensions*

* Dimensions not shown on request

WD [mm] 0,89 1,00 1,20 1,24 1,65 1,82 2,00 2,11 2,30 2,35 2,50 2,60 2,64 2,77 2,87 3,00 3,20 3,25 3,60 3,85 3,91 4,00 4,40 5,50 6,35 7,00
AD [inch] 0,035 0,048 0,065 0,072 0,083 0,093 0,104 0,109 0,113 0,126 0,128 0,154 0,250
[mm] [inch]
6,00
6,35 0,250
7,00
7,50
8,00
9,00
9,53 0,375
10,00
11,00
12,70 0,500
13,00
15,00
15,88 0,625
16,00
16,80
17,15 0,675
18,00
19,00
19,05 0,750
20,00
21,34 0,840
22,00
22,23 0,875
23,00
25,00
25,40 1,000
26,00
26,67 1,050
28,00
30,00
31,75 1,250
32,00
33,40 1,315
36,00
38,10 1,500
42,00
44,50 1,750

You have Questions?